A Re-Examination Of The Adams And Williamson Law Of Annealing

The adams and williamson law has been somewhat generally misinterpreted, in part because it has been generally extended over space instead of being confined to time. When restricted to what was actually observed, the law becomes intelligible and its seeming inconsistencies are straighten out.

Author
Fw Preston
Origin
Unknown
Journal Title
J.S.G.T 36 1952 287-296
Sector
Primary Papers
Class
PP 1507