Rating System Of Windows For Residential Buildings In Italy (In Italian)

Building energy consumption mostly depends on heat transfer and solar gain which occur through the windows. An iniative is illustrated for the introduction of a window rating system for the domestic residential building sector, aiming to enhance the Italian market of energy-efficient products. An appropriate use of this system will allow architectural engineers to lower energy consumption in residental buildings and consequently to reduce CO2 emissions.

Author
M Boschi Et Al
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 29 4 1999 169-182
Sector
Flat glass
Class
F 1033

Request article (free for British Glass members)

Rating System Of Windows For Residential Buildings In Italy (In Italian)
Riv Staz Sper Vetro 29 4 1999 169-182
F 1033
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.