Rate Controlled Debindering Of Glass Ceramic Composites

Green compacts of ceramics, glass ceramic composites & sinter glass ceramics contain different amounts of organic materials added as pressing aids or binders. Before sintering, these organics have to burn out completely. In oxidising atmospheres, the debindering process is mostly exothermic & therefore difficult to control. This uncontrolled heat production due to locally enhanced debindering & respective gas release may cause damages in the green compact microstructure. Therefore, debindering is usually operated with very low heating rates.({3K/min) which requires long processing times of many hours. In this paper we will show that it is possible to reduce the processing time for debindering dramatically by using the decomposition rate of the organic binder, detected by the weight loss of the sample, as a control factor for the furnace.

Author
S. Reisch Et Al.
Origin
Federal Institute For Materials Research And Testing (Bam), Germany
Journal Title
Advanced Materials Research Vols 39-40 (2008) 583-586
Sector
Glass Ceramics
Class
GC 712

Request article (free for British Glass members)

Rate Controlled Debindering Of Glass Ceramic Composites
Advanced Materials Research Vols 39-40 (2008) 583-586
GC 712
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.