Rapid Chemical Methods For The Analysis Of Glasses And Glassmaking Materials

Progress has been achieved by simplification of methods of decomposing the sample and of the classical procedures of analysis, elimination when possible of separation processes, and the use of highly selective reagents. These and other advances are reviewed.