The Rapid Analysis Of Fluorine In Glass By The Use Of Fluoride Ion Sensitive Electrodes

A rapid analysis for the direct determination of fluorine in glass using the Corning fluoride specific electrode without a prior separation of interfering ions is given. Among many buffer solutions, a 1M sodium citrate buffer solution was recommended for the analysis of fluorine in glass samples.

Author
M. Noshiro And Y. Jitsugiri