Raman Scattering Spectra And Optical Properties Of Tellurite Glasses And Crystalline Phases Containing Pb0 And Cd0

The glass forming region in the system Pb0-Cd0-Te02 was determined and the structure of glasses and crystalline phases were examined by Raman scatting spectra.

Author
T Komatsu & H Mohri
Origin
Nagaoka University Of Tech, Japan
Journal Title
Phys Chem Glasses 40 5 1999 257-263
Sector
Special Glass
Class
S 1766

Request article (free for British Glass members)

Raman Scattering Spectra And Optical Properties Of Tellurite Glasses And Crystalline Phases Containing Pb0 And Cd0
Phys Chem Glasses 40 5 1999 257-263
S 1766