Radiation-Optical Properties Of Iron-Containing Potassium-Aluminoborate Glass

Experimental studies on the radiation-optical properties of potassium aluminoborate glasses containing iron oxide, to ascertain the feasibility of obtaining prescribed radiation-induced tints in glass, are reported. Controllable tints from dark blue to yellow with varying degrees of darkening were produced.

Author
A N Salakhitdinov Et Al
Origin
Unknown
Journal Title
Glass And Ceramics 1989 46 3-4 166-170