Radiation Hardening Of Silica Glass Through Fictive Temperature Reduction

The aim of this article was to report the effects of y-radiation on type I Infrasil silica glass with different fictive temperatures, Tf, for harsh environment applications. Radiation-induced attenuation in the visible range is found to be much lower in low fictive temperature samples. Photoluminescence experiments show that glasses with higher fictive temperatures have a higher nonbridging oxygen hole centres defect concentration generated by irradiation.

Author
M Lancry Et Al
Origin
University De Paris Saclay, Orsay, France
Journal Title
Appl Glass Sci 8 2017 285-290
Sector
Special Glass
Class
S 4409

Request article (free for British Glass members)

Radiation Hardening Of Silica Glass Through Fictive Temperature Reduction
Appl Glass Sci 8 2017 285-290
S 4409
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.