Quinn Installs Xpar Infrared Systems

Quinn Glass is to gradually adapt its hot end to XPAR Vision's infrared technology. The companies have come to a first phase agreement that will see the Dutch company supply five Polysigma single camera unit systems. Three systems were installed earlier this year at Quinn's new glass container factory at Elton, and two units are scheduled for installation at the Derrylin plant in Northern Ireland. (whole item)