Quinn Glass Win Cobra Contract

Quinn Glass has won a 4y contract to be the sole supplier of glass for Cobra beer. The glassmaker will be the main contract packer for Cobra and will pack both the 330ml and 660ml bottles in six, 12 and 24 cluster pack formats. Quinn will manufacture the bottles at its sites in Derrylin, Northern Ireland, and Elton, Cheshire. However, as Cobra's volumes increase Quinn intends to move all glass production to its Elton site, where the bottles are filled. A spokesman said: "Quinn is delighted to welcome the Cobra contract, having brought the production of glass and the filling across from Poland." The company will supply the on and off-trade markets in the UK and the majority of Cobra's foreign markets.

Author
Un-named
Origin
Unknown
Journal Title
Packaging News 9 May 2009
Sector
Packaging Abstracts
Class
PA 424

Request article (free for British Glass members)

Quinn Glass Win Cobra Contract
Packaging News 9 May 2009
PA 424
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.