Quantum Size Effect And Energy Transfer In The System: Cds Nanoparticles And Tb(Iii) Ions In Oxide Xerogels

CdS nanoparticles have been prepared by a quaternary reverse micelle method. The size of the nanoparticles as controlled by changing the W(W=[H2O]/[CTAC]) molar ratio was in the quantum dot range. UV-Vis absorption and luminescence emission spectra of the CdS nanoparticles and materials consisting of the nanoparticles with Tb (III) ions incorporated into oxide xerogels show a quantum size effect. On other hand, for the materials there is observed an enhancement of emission intensity, owing to energy transfer from the excited CdS quantum dots to the emitting Tb(III). Additionally, a new effect, is described, namely the decreasing size of the CdS nanoparticles, that causes decrease of the emission intensity of Tb(III) ions and red shifting their bands.

Author
M Zalewska Et Al
Origin
University Of Gdansk, Poland
Journal Title
Physics & Chemistry Of Glasses June 2007 Volume 48 3 117-122
Sector
Special Glass
Class
S 3326

Request article (free for British Glass members)

Quantum Size Effect And Energy Transfer In The System: Cds Nanoparticles And Tb(Iii) Ions In Oxide Xerogels
Physics & Chemistry Of Glasses June 2007 Volume 48 3 117-122
S 3326