Quantum Cutting In Luminescent Glasses And Glass Ceramics

In the last decade, revolutions in photonic material design and large-area nanostructure fabrication have given researchers and technologists tools to enable a new era of ultrahigh-efficiency photovoltaics. Quantum cutting has received much attention as a potential approach to enhance the photovoltaic conversion efficiency of solar cell in the recent decades. In this article, the phenomena, mechanisms and design of the quantum cutting processes is reviewed, focusing on the promising applications of the transparent glasses and glass ceramic materials as the down-converter of solar spectrum. The authors also discuss the gaps between the current theoretical analysis and the practical applications of the quantum-cutting materials. To concave the negative effects of using the quantum-cutting materials as a down-converter on the front surface of the solar cell, much attention should be given to the choice of material and improvement of the material properties as well as the integration of photonic nanostructures and circuits on the solar cell.

Author
J Zhou Et Al
Origin
Zhejiang University, Hangzhou, China
Journal Title
Int J Appl Glass Sci 3 4 2012 299-308
Sector
Glass Ceramics
Class
GC 822

Request article (free for British Glass members)

Quantum Cutting In Luminescent Glasses And Glass Ceramics
Int J Appl Glass Sci 3 4 2012 299-308
GC 822
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.