Quantum Confinement Of Pbs Microcrystals In Glass

A microcrystalline PbS phase has been thermally produced from an oxide glass host. X-ray linewidth measurements have shown that the average particle size can be controlled in the range 8-30nm, depending on the thermal development schedule. Quantum confinement behaviour has been observed based on the measurement of sub-band structure of the absorption edge. Spectral shifts of the sub-bands were found to be consistent with the inverse square of the particle size, consistent with a quantum confinement origin. A lower-concentration PbSe phase has also been obtained from the same base-glass composition showing similar optical effects.

Author
N F Borrelli & D W Smith
Origin
Corning Inc, Ny, Usa
Journal Title
Corning Research 1994 189-195
Sector
Special Glass
Class
S 945

Request article (free for British Glass members)

Quantum Confinement Of Pbs Microcrystals In Glass
Corning Research 1994 189-195
S 945
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.