Quantitative Microprobe Analysis Of Sodium And Potassium In Glasses (In French)

The quantitative determination of sodium and potassium in glasses using the electron microprobe presents certain difficulties, but these may be largely overcome by choosing the appropriate standards and experimental conditions specially selected for the type of glass to be analysed.