Quantitative Characterisation Of Nuclei Formation By Raman Spectroscopy Of Lithium-Aluminosilicate Glass Ceramics Doped With Titania And Zirconia

Due to their nominal zero thermal expansion and high transparency, glass ceramics in the Li20-Al203-Si02 system found a variety of technical applications. Titania and zirconia are used as effective nucleating agents in parent glasses for heterogeneous nucleation of high-quartz solid solutions crystals. The catalyzing role of these oxides is explained by phase separation and subsequent crystallisation of ZrxTi(2-x)O4 crystals under thermal treatment.

Author
F Gabel Et Al
Origin
Fraunhofer Institut, Germany
Journal Title
Proc Icg Extended Abstracts 2 2001 189-190
Sector
Glass Ceramics
Class
GC 547

Request article (free for British Glass members)

Quantitative Characterisation Of Nuclei Formation By Raman Spectroscopy Of Lithium-Aluminosilicate Glass Ceramics Doped With Titania And Zirconia
Proc Icg Extended Abstracts 2 2001 189-190
GC 547
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.