Quantitative Analysis Of Glass By Emission Spectrography; Six-Element Survey

The use of this technique for analysing small (1mg) fragments of glass is described. The contents of Al,Ba,Ca,Fe,Mg and Mn in 200 samples were used to classify the samples as sheet, tableware or container glass, and to discriminate between glasses closely similar in refractive index.