The Quality Of Mixed Cullet

About one million tons of glass cullet are used yearly by the Italian glassworks for the production of coloured container glass, and it often is the main component of the batch. A description is given of a cullet quality parameters that must be closely controlled by glass producers. Different inorganic contaminants are examined, which can cause the formation of stones in the final product. The parameters affecting the redox state of the melt and its influences on the final glass colour are discussed, with particular reference to organic contaminents and the redox state of the cullet. The negative effects of heavy metals and halids on the quality of the final glass (for food containers) and waste gases are also discussed.

Author
R Falcone Et Al
Origin
Stazione Sperimentale, Italy
Journal Title
Rivista Stazione 2 2003 35-39
Sector
Container glass
Class
C 3404

Request article (free for British Glass members)

The Quality Of Mixed Cullet
Rivista Stazione 2 2003 35-39
C 3404
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.