Quality Feldspar Production At Cine Akmaden

Feldspars are indispensable raw materials for ceramics and glass industries due to their alkali and alumina contents. Although the earth's crust mainly consists of feldspar, being 25.6% in various grades as rock forming minerals, hitherto only some, namely albite, orthoclase and microcline have been exploited for glass and ceramic making.