[Quality Control] Smart Temperature Sensors For Glass Improve Repeatability

Advances in microelectronics have increased the capability of optical temperature sensors giving improved repeatability, accuracy and speed. These smart sensors can also provide new benefits when measuring dynamic processes by isolating critical process data from a stream of rapidly varying process measurements.