Quality Control In The Flat Glass Industry

Methods for automatic inspection of float glass are reviewed briefly.

Author
F.B. Slabodsky
Origin
Unknown
Journal Title
Glass 1984 61 (11) 379-380, 382
Sector
Primary Papers
Class
PP 180