Quality Assurance Of Sintered Refractories Through Nondestructive Testing With Microwaves

For quality assurance of refractories for the glass industry an early nondestructive test is required. A possibility for nondestructive testing, especially in green products, is given by the transition of microwaves, as this requires no coupling medium like water. In this work, some basic physical characteristics were measured which determine microwave absorption through refractories and flaw detection. For different refractories the dielectric constant, specific attenuation coefficient as well as dependence of the attenuation on the frequency were determined. It is shown that a high dielectric constant improves the deteciton of flaws.

Author
H Dannheim & H Hadrich
Origin
Inst Werkstoffwissenschaften & Universitat Erlangen-Nurnberg
Journal Title
Glastech Ber Glass Sci Technol 71 8 1998 223-229
Sector
Refractories
Class
R 286

Request article (free for British Glass members)

Quality Assurance Of Sintered Refractories Through Nondestructive Testing With Microwaves
Glastech Ber Glass Sci Technol 71 8 1998 223-229
R 286
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.