Protection Offered By Glass Floors Steps Up A Level

Glazeguard has created the Triple-Lite Firefloor system incorporating Pilkington Pyrostop. At 1m x 3m for a single panel, it is the largest fire-resistant floor that has been tested & approved to current British & new European standards. It offers incredible strength & durability & provides protection for over 1-hr for both integrity & insulation. It allows crucial time for the safe evacuation of people & prolongs protection to the building fabric. As a single layer glass-to-glass butt-jointed system, the new product is suitable for both domestic & commercial glass floor applications. It provides all the aesthetic qualities associated with glass floors, allowing natural light transmission and bright, airy spaces, while from a practical point of view it is robust, strong & provides safe & secure environments.

Author
Un-named
Origin
Unknown
Journal Title
Theglazine News 27/09/05
Sector
Flat glass
Class
F 1882

Request article (free for British Glass members)

Protection Offered By Glass Floors Steps Up A Level
Theglazine News 27/09/05
F 1882
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.