Protection Against Rat-Holes

Lubisol Engineering Co. is offering its Si-Seal Crown Design technology to glass makers to guard against rat-holing in silica crowns, a special problem with oxy-fuel. The main feature of Si-Seal Crown Design is a special protective layer placed between the main crown and the thermal insulation of the furnace. The protective layer hermetically seals the crown and prevents the passing of hot aggressive gases, thus reducing or eliminating the rat-holing. The protective layer forms a strong adhesive bond towards the silica bricks at temperatures up to 1600 deg C, and provides high corrosive resistance. Coefficient of expansion is equal or very close to that of silica - 1.28%. The technique is suitable for application on a cold crown, during or after heat-up, and also for hot repair. Please contact Lubisol Eng by fax on: (USA) +516 329 6674.

Author
Un-named
Origin
Unknown
Journal Title
Am Glass Review 119 4 Jan-Feb 1999 17
Sector
Refractories
Class
R 317

Request article (free for British Glass members)

Protection Against Rat-Holes
Am Glass Review 119 4 Jan-Feb 1999 17
R 317
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 19 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.