Properties - Structure Relations Of Zn0-Pb0-B203 Glasses

Density, Vickers' hardness, transformation temperature and thermal expansion of xZn0.2xPb0.(100-3x)B203 glasses have been investigated as a function of composition. Variations of the properties around 50 mol% (Zn0+Pb0) are attributed to nonbridging oxygen ions formed in the borate matrix. Parameters are given to calculate the density in the Zn0-Pb0-B203 glasses. Results indicate that the fraction of modifier oxide given from a Zn0 content is lower than that given from an equal Pb0 content.

Author
H Doweidar Et Al
Origin
Mansoura University, Egypt
Journal Title
Phys Chem Glasses 40 5 1999 252-256
Sector
Special Glass
Class
S 1765

Request article (free for British Glass members)

Properties - Structure Relations Of Zn0-Pb0-B203 Glasses
Phys Chem Glasses 40 5 1999 252-256
S 1765
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.