Properties Of Silica Glass Doped With Titanium Oxide

The features of anomalous behaviour of silica glass doped with titanium oxide are discussed. The low thermal expansion of silica glass is considered on the base of the idea about polymorphous transformations in meta stable-glass structures. The analogy of these transformations to structural transitions of martensite type in metallic alloys is assumed. The effect of TiO2-doping on the structure and the intrinsic strength of silica glass fibres is studied. The structural (intrinsic) strength has been found to decrease by about 15% compared to that of non doped silica glass. This decrease of strength is assumed to be accounted for the incorporation of a part of titanium ions into glass structure with six fold coordination resulting in weakening the connectivity of a glass anionic network.

Author
V. Pukh Et Al
Origin
Loffe Physical-Technical Institute, St Petersburg, Russia
Journal Title
Advanced Materials Research Vols 39-40 2008 153-158
Sector
Special Glass
Class
S 3399

Request article (free for British Glass members)

Properties Of Silica Glass Doped With Titanium Oxide
Advanced Materials Research Vols 39-40 2008 153-158
S 3399