Properties Of Porous Glasses After Impregnation With Caesium And Potassium Ions

Porous glasses, the products of leaching of heat treated alkali borosilicate glasses, are very useful materials for impregnation with different ions. The results of measurements of electrical and optical properties of the porous glass after impregnation with caesium and potassium ions are presented. The measurements were performed successively after each stage of the technological process.

Author
E Rysiakiewica-Pasek & K Marczuk
Origin
Tech University Of Wroclaw, Poland
Journal Title
Phys & Chem Glasses 35 4 1994 164-168
Sector
Special Glass
Class
S 814

Request article (free for British Glass members)

Properties Of Porous Glasses After Impregnation With Caesium And Potassium Ions
Phys & Chem Glasses 35 4 1994 164-168
S 814
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.