Properties Of Cao-Tio2-Si02 Glasses

Glasses in the system CaO-TiO2-SiO2 with TiO2 content of up to 30 mol% were prepared. The glasses were characterised thermally, chemically and mechanically. In all the compositions studied, a strong phase separation was observed by transmission electron microscopy, with increased droplet size as the TiO2 content increased. As is to be expected, the thermal expansion coefficients were lower than those of conventional soda-lime glasses. The incorporation of TiO2 into the glass network enhanced microhardness and toughness.

Author
M A Villegas Et Al
Origin
Inst De Ceramica Y Vidrio, Madrid, Spain
Journal Title
Glass Technology 35 6 1994 276-280
Sector
Special Glass
Class
S 829

Request article (free for British Glass members)

Properties Of Cao-Tio2-Si02 Glasses
Glass Technology 35 6 1994 276-280
S 829
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.