Properties Of Bao-B2O3-P2O5 Glasses For Active Optical Fibres

Viscosity in the range of 10 7 and 10 11Pas was measured by a penetration method for barium phosphate and borophosphate glass melts in a series of xB2O3-(100-x)Ba(PO3)2 where x=0-12mol%. The viscosity at a certain temperature increases with increasing B2O3 concentration. The variation of viscosity with B2O3 concentration is qualitatively related to glass structure reported in previous studies. The immersion test into distilled water for glass plates reveals that B2O3 addition degrades water durability. The microstructure observation reveals the precipitation of many nano-sized particles at the immersed surface of a barium borophosphate glass. No spectral change of Nd3+ absorption was observed in between binary barium phosphate and ternary barium borophosphate glasses due to the site selectivity of Nd3+ ions with PO4 networks.

Author
H Takebe Et Al
Origin
Japan
Journal Title
Physics & Chemistry Of Glasses June 2007 Volume 48 3 113-116
Sector
Special Glass
Class
S 3325

Request article (free for British Glass members)

Properties Of Bao-B2O3-P2O5 Glasses For Active Optical Fibres
Physics & Chemistry Of Glasses June 2007 Volume 48 3 113-116
S 3325
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.