Lithium germanate glasses with 0-30 mol% Li2O were prepared amd measurements made of refractive index, thermal expansion coefficient, glass transformation temperature, dc electrical conductivity, crystallisation temperature and infrared spectra.

Author
J E Shelby, J Ruller
Origin
Alfred University
Journal Title
Phys Chem Glasses 1987 28 6 262-268