Progress In Reducing Energy And Co2 By Combining A Batch/Cullet Preheater With An Oxy-Fuel Fired Furnace

Two oxy-fuel fired furnaces equipped with batch/cullet preheaters have demonstrated specific fuel consumptions of 2.9-3.2 GJ/ton for container glass with 50-60% cullet, or around 30% fuel savings over state-of-the-art regenerative furnaces. Praxair is currently developing an advanced batch/cullet preheater which is projected to reduce the specific fuel consumption further to 2.65 GJ/ton and specific CO2 emissions to 237 KG/ton. Experiences from past batch/cullet preheater installations are reviewed and progress on the development of this advanced system is reported.

Author
H Kobayashi Et Al
Origin
Praxair Inc
Journal Title
Gmpa 3/2007 86-89
Sector
General
Class
G 3327

Request article (free for British Glass members)

Progress In Reducing Energy And Co2 By Combining A Batch/Cullet Preheater With An Oxy-Fuel Fired Furnace
Gmpa 3/2007 86-89
G 3327
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.