Progress In Glass Structure Determination

Progress in determining partial distribution functions by neutron and anomalous X-ray scattering is reviewed. Complementary results from EXAFS, MASNMR and LFN spectroscopies are also discussed.

Author
J Zarzycki
Origin
University Of Montpellier
Journal Title
Riv Staz Sper Vetro 1990 20 5 13-20