Profile Analysis Of Quadrupole Broadened Nuclear Magnetic Resonance Spectra Of Glasses

A method is presented which retrieves structural information from (magic angle spinning) nuclear magnetic resonance spectra in glasses broadened by second order quadrupolar effects.