Production Of Iron-Containing Crystalline Glazes

Results of production of crystalline glaze with a decorative aventurine effect are given. Synthesis of glaze was performed based on frit containing Na2O, B2O3, and Sio2 using the simple-lattice method of experiment design.It is established that the aventurine effect is caused by hematite crystals