Production Of Foam Glass From Glass Waste (In Italian)

This paper illustrates the possibility of using recycled glass to obtain foam glass as an added value product. Soda-lime glass cullet, lead and barium silicate glasses from cathode ray tubes, and a silicate industrial waste from the polishing of porcelain stoneware were used as starting materials to produce cellular glasses. The control of the cellular structure and therefore the tailoring of the expected final material properties were achieved by varying the processing parameters.

Author
G Brusatin Et Al
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 35 4 2005 17-26
Sector
Special Glass
Class
S 3239

Request article (free for British Glass members)

Production Of Foam Glass From Glass Waste (In Italian)
Riv Staz Sper Vetro 35 4 2005 17-26
S 3239
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.