Product Vs Corporate Carbon Footprint: Some Methodological Issues. A Case Study And Review On The Wine Sector

Carbon footprint (CF) is nowadays one of the most widely used environmental indicators. Six main methodological issues to take into account when collecting corporate data to be used for PCF studies were postulated and discussed in the present paper: fugitive emissions, credits from waste recycling, use of “equivalent factors”, reference flow definition, accumulation and allocation of corporate values to minor products. A big project with 18 wineries, being wine one of the most important agri-food products assessed through CF methodologies, was used to study and to exemplify these 6 methodological issues. The methodology discussed in this paper for the wine case study is widely applicable to any other product or industrial activity.

Author
A Navarro Et Al
Origin
Unknown
Journal Title
Sci Of The Total Env March Vol 581-2 2017 722-733
Sector
Container glass
Class
C 5832a

Request article (free for British Glass members)

Product Vs Corporate Carbon Footprint: Some Methodological Issues. A Case Study And Review On The Wine Sector
Sci Of The Total Env March Vol 581-2 2017 722-733
C 5832a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.