Processing Effects On The Surface Composition Of Glass Fibre

In this study, differences in the surface composition of commercial glass fibre have been characterized as a function of process. The two processes studied were flame attenuation, a high-temperature combustion-assisted process, and continuous filament drawing through a bushing. The techniques used to determine the surface compositions were TOF-SIMS and XPS; the presence of a very thin, boron-depleted silica-enriched layer on the flame-attenuated fibres was most significant. Thermodynamic modeling of the equilibrium vapor pressures at the surface, during fiberization, showed significant differences in the behaviour of Na, B and F species in the two processes. To further test the models, glass fibres were produced under more closely controlled conditions in a laboratory-scale flame attenuation system.

Author
M N Palmisiano Et Al
Origin
Pennsylvania State University, Usa
Journal Title
J Am Ceram Soc 83 10 2000 2423-2428
Sector
Glass Fibre
Class
GF 260

Request article (free for British Glass members)

Processing Effects On The Surface Composition Of Glass Fibre
J Am Ceram Soc 83 10 2000 2423-2428
GF 260
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.