Process Prototyping - Physical Model Of The Glass Pressing Process

A physical model of the glass pressing process has been developed based on the theory of dimensional analysis. The main objective of this approach was to set up an equivalent model process operating on a significantly lower temperature level than the original pressing process. Therefore, a model glass had to be found that showed the same thermoviscous behaviour as the glass used in the original production. It is proved mathematically that at least one type of nitrate glass matches these requirements. Initially, the process under examination had to be described dimensionlessly. Starting from this dimensionless base, scale equations could be derived according to the model laws of dimensional analysis.

Author
H-Jungen Trossin
Origin
Technische Universitat Munchen, Germany
Journal Title
Glastech Ber Glass Sci Technol 72 4 1999 112-117
Sector
Special Glass
Class
S 1631

Request article (free for British Glass members)

Process Prototyping - Physical Model Of The Glass Pressing Process
Glastech Ber Glass Sci Technol 72 4 1999 112-117
S 1631
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.