Probing Glass Oxidation States Using Fluorescence Spectroscopy

Spectroscopic techniques have been used to identify oxidation states in manufactured pieces for some time. Light used as a signal is potentially more reliable since it is not prone in the same way, to interferences that can affect electrical signals. While using light at low temperature has been common practice, the emissivity of glasses at high temperature has restricted its use. Absorbance spectroscopy is the commonly used method. However, reasonable concentrations of absorbing species are required for identification, which quantitatively depends on the geometry of the sample. Optical absorption measurements for glass samples from ambient temperatures up to 1300 deg C have been made. The ferrous band at 1050nm was the only species measured, and therefor the ferric/ferrous ratio could not be determined with changing temperature.

Author
A G Clare & D J Ames
Origin
Nyscc At Alfred University, Usa
Journal Title
The Glass Researcher 10 1 2000 15-16, 19
Sector
Special Glass
Class
S 2093

Request article (free for British Glass members)

Probing Glass Oxidation States Using Fluorescence Spectroscopy
The Glass Researcher 10 1 2000 15-16, 19
S 2093
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.