Printed Glass In The Manufacture Of Pharmaceutical Packaging (Italian)

The increase in the use of treated soda-lime glass (Type II) is discussed.

Author
A Biavati
Origin
Unknown
Journal Title
Rass Del' Imballaggio 1988 9 33-34 26-27
Sector
Container glass
Class
C 224