Principles Of The Polyliquid Process For Thermal Toughening Of Glass

Measurement of heat transfer functions of a polyliquid system by use of a simple silver probe has been demonstrated to take little time and no sample preparation. Study of the trends of influence for any polyliquid parameter, measurement of heat transfer and stress computation requires considerably less experimental effort than preparing, quenching and testing a statistically significant number of glass specimens.