Primary Stabilisation Factor Of The Corrosion Of Historical Glasses: The Gel Layer

Leached gel layers of variable thickness and composition, mostly crisscrossed by cracks and fissures, are built during long-term exposure of historical glasses. Depending on the glass composition as well as on the environmental conditions the gel layers show various shapes. They can be characterised by microprobe investigations, though photographs of the cross-sections in vertical plane to the corroded surface as well as determinatoin of the chemical composition.

Author
W Muller Et Al
Origin
Bundesanstalt Fur Materialforschung Und-Profumg, Berlin
Journal Title
Glastech Ber Glass Sci Technol 68 9 1995 285-292
Sector
Flat glass
Class
F 505

Request article (free for British Glass members)

Primary Stabilisation Factor Of The Corrosion Of Historical Glasses: The Gel Layer
Glastech Ber Glass Sci Technol 68 9 1995 285-292
F 505
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.