Primary And Secondary Phase Separation In Cdf2-Lif-Alf3-Pbf2 Glasses

Occurrence of primary and secondary phase separation in the CdF2-LiF-AlF3-PbF3 glass systems has been observed. A pseudobinary model explaining the occurrence of these phenomena is presented.