Pressure Testing Of Non-Pressure Ware

Many have questioned whether it makes sense to use a pressure test as a means to monitor & manage the quality performance of non-pressure ware when it is not expected to withstand sustained internal pressure loading. This article answers the question by showing that, in general, the response of pressure ware & non-pressure ware are the same (excluding unusual sizes/shapes of some non-pressure ware).

Author
M W Davis
Origin
Unknown
Journal Title
Glass Worldwide May-June 2007 58, 60-62