The Present Scenario Of Non-Recovery Coke Ovens In India And Development Of New Refractory Technology

The present status of coke making through the use of non-recovery coke ovens (NRCO) has been described. The main features and key characteristics of this type of oven have also been highlighted. The authors own contribution in development of innovative refractory technology for improved performance of this type of coke oven has also been elucidated.

Author
S.N. Laha
Origin
Natasha Ceramic And Consultancy Services
Journal Title
Trans Indian Ceramic Society, Vol 65, No 2, Apr-Jun 2006
Sector
Refractories
Class
R 762

Request article (free for British Glass members)

The Present Scenario Of Non-Recovery Coke Ovens In India And Development Of New Refractory Technology
Trans Indian Ceramic Society, Vol 65, No 2, Apr-Jun 2006
R 762
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.