Preparation, Nanostructure And Properties Of Indium Tin Oxide (Ito) Films On Glass Substrates. Part 1. Preparation And Nanostructure

Indium tin oxide (ITO) films of xSn02.(100-x)In203 compositions with x=0,6,9,11,14 mol% were prepared by sol-gel dip coating on glass substrates. By using diand triethanolamine as stabilisers and dry nitrogen as an atmosphere, it was possible to prepare a very stable solution for dip coating in air.

Author
J Liu Et Al
Origin
Unknown
Journal Title
Phys Chem Glasses 40 5 1999 277-281