Preparation Of Nanocrystalline Zro2 Powder Via A Chemical Route

Nanocrystalline ZrO2 powder was prepared through a chemical route via a reaction between a soluble salt within an organic template in various ratios at a carbonization temperature of 200 degrees C. The homogenization of the nanopowder was assisted by milling the charcoal precursor in a non polar solvent for 24 hours, followed by calcining at 800 degrees C and 1100 degrees C. X-ray diffraction (XRD) analysis results show that zirconia nanopowder produced has crystallite sizes of about 26-31 nm and 46-50 nm whose major crystal phase is m-ZrO2 for calcinations at 800 degrees C and 1100 degrees C, respectively. Increasing the organic template concentration reduced the particle and crystallite size, while the elevation of the calcination temperature enlarges the particle and crystallite size.

Author
R Septawendar Et Al
Origin
Unknown
Journal Title
Journal Of The Australian Ceramic Society 48 1 2012 12-20
Sector
Special Glass
Class
S 3854

Request article (free for British Glass members)

Preparation Of Nanocrystalline Zro2 Powder Via A Chemical Route
Journal Of The Australian Ceramic Society 48 1 2012 12-20
S 3854
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.