Preparation Of Mixed Alkali Multicomponent Phosphate Glasses And Some Studies On Their Thermomechanical And Optical Properties

The 40P2O5.12Al2O3.6BO3.9PbO.xNa2O.(33-x)K2O series of phosphate glasses have been prepared using the conventional melt quenching technique.

Author
K V Shah Et Al
Origin
Bhabha Atomic Research Centre, Mumbai
Journal Title
Phys Chem Glasses 46 3 2005 274-278
Sector
Special Glass
Class
S 2987

Request article (free for British Glass members)

Preparation Of Mixed Alkali Multicomponent Phosphate Glasses And Some Studies On Their Thermomechanical And Optical Properties
Phys Chem Glasses 46 3 2005 274-278
S 2987