Preparation Of Lio2-Sio2 Gels And Glasses By Sol-Gel Methods

Lithium silicate gels with lithia contents from 5 to 40 mol% were prepared by several sol-gel methods. Structural development was investigated by nuclear magnetic resonance.

Author
W Beier, U Wellbrock, G H Frischat
Origin
Technische Universitat Clausthal
Journal Title
Glastech Ber 1990 63 6 163-171