Preparation Of Cobalt- And Fluorine-Doped Barium Hexaferrite By The Glass Synthesis Method

Doped barium hexaferrite has been prepared by the glass synthesis method, the fluorine improving the pouring of the melt and the crystallisation of the glass while the cobalt decreases the coercive force.