Preparation Bts And Mas Glass-Ceramic As Pane Material For Light Scattering And Depolarization

BTS (Ba0-Ti02-Si02) and MAS MgO-Al203-Si02) glass-ceramics have been prepared as a pane material with light scattering and depolarization due to their special crystalliztaion features. The experimental results indicate that the crystallization process is controllable and could be managed. The measured properties (surface hardness, constant of thermal expansion and optical characteristics) could meet the requirement of replacing natural materials.

Author
W Wei Et Al
Origin
Wuhan University Of Technolgoy, China
Journal Title
Proc Xvii Int Cong Glass, Vol 7, Beijing 1995, 144-148
Sector
Glass Ceramics
Class
GC 312

Request article (free for British Glass members)

Preparation Bts And Mas Glass-Ceramic As Pane Material For Light Scattering And Depolarization
Proc Xvii Int Cong Glass, Vol 7, Beijing 1995, 144-148
GC 312
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.